GATE Assistant

Past questions › Metallurgical Engineering › GATE 2024

GATE 2024 · MT · NAT · 2 marks · Metallurgical Thermodynamics › Electrochemistry & Potential-pH Diagrams

GATE 2024 Metallurgical Engineering question: The cupric ion (Cu 2+ ) concentration in the electrolyte (at 298 K) required to make the…

The cupric ion () concentration in the electrolyte (at 298 ) required to make the potential of pure copper equal to 0.17 is _______ –. . (Round off to two decimal places).

Gas constant

Faraday’s constant (of electrons)

Standard reduction potential of Cu,

Show answer

Official answer: 1.6 to 1.9

Practise this question with exam-style marking