GATE 2024 TF Engineering Sciences question: Three melt-spun fibre samples A, B and C produced from same polymer under different…
Three melt-spun fibre samples A, B and C produced from same polymer under different conditions are found to have densities 1.10 g/cm, 1.15 g/cm and 1.20 g/cm, respectively. If the mass fraction based degree of crystallinity () of A and C is 0.45 and 0.75, respectively, then for B (rounded off to 2 decimal places) is _________________.
Show answer
Official answer: 0.59 to 0.63