Match the casting defects in Column I with the characteristic features in Column II.

Column I Column II
P. Misrun 1. Penetration of liquid metal behind surface layer of sand moulds
Q. Expansion scab 2. Metal solidifies prematurely in the mould and some sections of the casting are not filled
R. Pin holes 3. Cracking because of restraint to contraction in certain areas of the casting during solidification and cooling to room temperature
S. Hot tearing 4. Evolution of gases during solidification resulting in porosity
  1. (A)

    P – 2, Q – 4, R – 3, S – 1

  2. (B)

    P – 1, Q – 3, R – 2, S – 4

  3. (C)

    P – 1, Q – 2, R – 4, S – 3

  4. (D)

    P – 2, Q – 1, R – 4, S – 3

Show answer

Official answer: D