GATE 2025 Metallurgical Engineering question: For a component fabricated from an alloy A with plane strain fracture toughness, K IC =…
For a component fabricated from an alloy A with plane strain fracture toughness, = 50 MPa m, fracture was observed to take place at a crack length of 0.4 mm at a tensile service stress of .
If the same component is instead fabricated from alloy B with = 75 MPa m, the crack length at which a similar crack geometry will result in fracture (under identical tensile service stress of ) is ______ mm (rounded off to one decimal place).
Show answer
Official answer: 0.9