In the first heating cycle of a differential scanning calorimetry (DSC) experiment, an as-spun Nylon 6 fibre showed an enthalpy change of 40 J/g during cold crystallization and an enthalpy change of 150 J/g during melting. If the heat of fusion of 100% crystalline Nylon 6 is 240 J/g, the percentage degree of crystallinity of as-spun Nylon 6 fibre (rounded off to 1 decimal place) is __________.

Show answer

Official answer: 45 to 46