GATE Assistant

Past questions › Mining Engineering › GATE 2026

GATE 2026 · MN · MCQ · 1 mark · Geomechanics and Ground Control › Geotechnical Properties & Rock Mass Classification

GATE 2026 Mining Engineering question: In a Slake Durability Index (SDI) test, a rock sample of 500 g undergoes two standard…

In a Slake Durability Index (SDI) test, a rock sample of 500 g undergoes two standard cycles of wetting and drying. The mass of the sample retained after the test is 400 g. The SDI of the sample, in %, is

  1. (A)

    10

  2. (B)

    40

  3. (C)

    20

  4. (D)

    80

Show answer

Official answer: D

Practise this question with exam-style marking

Discussion

No discussion yet.

Join the discussion