GATE 2026 Metallurgical Engineering question: Iron powder is compacted at room temperature to 75% of its theoretical density. The…
Iron powder is compacted at room temperature to 75% of its theoretical density. The as-pressed iron compact is sintered in inert-gas atmosphere at 1200 °C to 90% of its theoretical density. Assuming isotropic shrinkage, the linear shrinkage (in percent) undergone by the iron compact during sintering (rounded off to one decimal place) is ________________ %
Show answer
Official answer: 5.8 to 6.1