GATE Assistant

Past questions › Metallurgical Engineering › GATE 2026

GATE 2026 · MT · NAT · 2 marks · Physical Metallurgy › Diffusion in Solids

GATE 2026 Metallurgical Engineering question: During carburizing of a steel, the surface concentration is kept constant at 1.4 wt.%…

During carburizing of a steel, the surface concentration is kept constant at 1.4 wt.% carbon. Diffusivity of carbon for the steel at 950 °C is m/s. At 950 °C, the time required to carburize the steel with an initial composition of 0.2 wt.% carbon to 0.8859 wt.% carbon at a depth of 0.2 mm is ______________ seconds (approximate to the nearest integer).

Use the nearest value of the error function from the table given below for your calculation.

z erf (z)
0.3 0.3268
0.4 0.4284
0.5 0.5205
Show answer

Official answer: 990 to 1010

Practise this question with exam-style marking

Discussion

No discussion yet.

Join the discussion